17-4 PH is a martensitic, chromium-nickel-copper precipitation-hardening stainless steel. 17-4PH Stainless Steel Plate is capable of attaining a wide range of strength and toughness properties depending on the precipitation or aging temperature used in hardening. 17-4PH SS Plate is valuable combination of high strength, good corrosion resistance and toughness in both base metals and welds gives designers opportunities to add reliability to their products while simplifying fabrication and often reducing costs. High strength is maintained to approximately 600F (316C). This material has good resistance to stress corrosion cracking in the lower strength conditions.
Inventory Size Range:
The technical data provided is for information only and not for design purposes. It is not warranted or guaranteed
Element | Percent By Weight Type 17-4ph | |
C | Carbon | 0.07 maximum |
Mn | Manganese | 1.00 maximum |
P | Phosphorus | 0.04 maximum |
S | Sulfur | 0.03 maximum |
Si | Silicon | 1.00 maximum |
Cr | Chromium | 15.00 - 17.50 |
Ni | Nickel | 3.00 - 5.00 |
Cu | Copper | 3.00 - 5.00 |
Nb | Columbium | 0.15 - 0.45 |
Common Applications of 17-4PH Stainless Steel Plate:
17-4PH Physical Properties:
Temperature Range | Coefficients | ||
C | F | m/mC | in/in/F106 |
21-93 | 70-200 | 10.8 | 6 |
21-204 | 70-400 | 10.8 | 6 |
21-316 | 70-600 | 11.2 | 6.2 |
21-427 | 70-800 | 11.2 | 6.3 |
Thermal Conductivity (H 900 Condition)
Temperature Range | W/mK | Btu/(hr/ft/in/F) | |
C | F | ||
149 | 300 | 17.9 | 124 |
260 | 500 | 19.5 | 135 |
460 | 860 | 22.5 | 156 |
482 | 900 | 22.6 | 157 |
Electrical Resistivity (Annealed Condition)
Microhm-cm: 98
Mechanical Properties and Yield Strength 17-4PH Stainless Steel - Cold Flattened (Annealed)